Name: Alloy Steel Pipe

WhatsApp:+8617663729118

E-mail:sales01@jiugangsteelgroup.com

Hastelloy C-22 Stainless Steel Pipe Tube
Hastelloy C-22 Stainless Steel Pipe Tube
Hastelloy C-22 Stainless Steel Pipe Tube
Hastelloy C-22 Stainless Steel Pipe Tube
Hastelloy C-22 Stainless Steel Pipe Tube
Hastelloy C-22 Stainless Steel Pipe Tube
Brand Name:Jiugang
Model Number:Hastelloy C-22 Stainless Steel Pipe Tube
Certification:ISO;CE
Minimum Order Quantity:3
Packaging Details:Waterproof paper+ wooden pallet or as customers' requirement
Delivery Time:7-15 days
Payment Terms:T/T or L/C at sight.


Quick Detail

Hastelloy C- 22, also known as alloy C22, is a highly adaptable austenitic nickel-chromium-molybdenum-tungsten alloy with higher resistance to pitting, crevice corrosion and stress corrosion cracking. High chromium contents have excellent resistance to oxidizing mediators, while molybdenum and tungsten contents have very good resistance to reducing mediators. This nickel steel alloy likewise has excellent oxidation resistance to aqueous media consisting of wet chlorine and mixtures containing nitric acid or oxidizing acids with chloride ions.

Hastelloy C22 is a heat-resistant woven wire mesh alloy known for its ability to hold its integrity when subjected to extreme temperatures. When looking at woven wire mesh, hastelloy c22 typically consists of a combination of chromium, molybdenum, nickel, and tungsten.


Specifications
Product NameHastelloy C-22 Pipe
Outer DiameterRound Pipe4mm-200mm
Square Pipe10*10mm-100*100mm
Rectangular Pipe10*20mm-50*100mm
Wall Thickness0.6mm-6.0mm
Length1-6 meters, Length can be customized
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBlack, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.
CertificateISO, SGS, BV
Production TechnologyHot Rolling, Cold Rolling
Mechanical Properties
Tensile Strength (ksi)0.2% Yield Strength (ksi)Elongation% in 2 inches
1004545

Physical Performance
UnitsTemperature in°C
Density8.69 g/cm³24°C
Specific Heat0.093 Kcal/kg.C52°
Melting Range1357-1399°C-
Modulus of Elasticity205.5 KN/mm²-
Electrical Resistivity113.7 µΩ.cm24 °
Coefficient of Expansion12.4 µm/m °C24-93°
Thermal Conductivity10.1 w/m-° K48°




Chemical Composition
CSiPSVCrMnFeCoNiMoW
0.015 max0.08 max0.02 max0.02 max0.35 max20.0 - 22.50.50 max2.0-6.02.5 maxRemainder12.5 - 14.52.5 - 3.5