Alloy Steel Plate

bimg

Project Information

Name: Alloy Steel Plate

WhatsApp:+8617663729118

E-mail:sales01@jiugangsteelgroup.com

Nickel Alloy 200 201 Plate
Nickel Alloy 200 201 Plate
Nickel Alloy 200 201 Plate
Brand Name:Jiugang
Model Number:Nickel Alloy 200 201 Plate
Certification:ISO;CE
Minimum Order Quantity:3
Packaging Details:Waterproof paper+ wooden pallet or as customers' requirement
Delivery Time:7-15 days
Payment Terms:T/T or L/C at sight.


Quick Detail

Nickel 200 and 201 plate offer outstanding corrosion resistance to caustic soda and other alkalis. They perform best in reducing environments but can also be used under oxidizing conditions when a passive oxide film is formed. They are used in aerospace, chemical and petrochemical processing, food processing, and marine and water treatment applications. Nickel 200 and 201 are both highly ductile across a wide temperature range and can be easily welded and processed by standard shop fabrication practices.


Specifications
Product NameNickel Alloy 200 201 Plate
Thickness0.3mm-200mm
Length2000mm, 2438mm, 3000mm, 5800mm, 6000mm, 12000mm, etc.
Width40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc.
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBA, 2B, NO.1, NO.4, 4K, HL, 8K, etc.
CertificateISO, SGS, BV
Production TechnologyHot Rolling, Cold Rolling


Mechanical Properties

Nickel 200/201, Typical Values at 70°F (21°C), Plate—Hot Rolled, Annealed

Yield Strength0.2% OffsetUltimate TensileStrengthElongationin 2 inchesHardness
ksiMPaksiMPa%Brinell(3000-kg)RockwellB
Nickel 20015–40105–27555–80380–55060–4090–14045–73
Nickel 20112–3583–24050–70345–48560–40

Physical Performance
UnitsTemperature in°C
Density0.321 lbs/in38.89 g/cm3
Specific Heat0.109BTU/lb-°F (32—212°F)456 J/kg-°K (0—100°C)
Modulus of Elasti        city 78°F (26°C)29.7 x 103 ksi205 GPa (20°C)
Thermal Conductivity 212°F (100°C)463 BTU-in/ft2-h-°F66.5 W/m-°C
Melting Range2615 – 2635°F2615 – 2635°F
Electrical Resistivity58 Ohm-circ mil/ft at 70°F0.096 µΩ/m at 20°C


Chemical Composition

Weight % (all values are maximum unless a range is otherwise indicated)

ElementNickel 200Nickel 201
Nickel (plus Cobalt)99.0 minimum99.0 minimum
Copper0.250.25
Iron0.400.40
Manganese0.350.35
Carbon0.150.02
Silicon0.350.35
Sulfur0.010.01